*Material
Surface layer: BOPP
Glue layer: EVA adhesive
*Specification
Gloss
Matt
*Process parameter:
*Directions for using BOPP thermal laminating film:
Normal process temperature is 90c-105c, roller pressure and temperature vary with different types of paper, ink and machines.
When using the film for the first time or do other treatment, try a small volume before mass laminating.
Make sure the ink is dry before laminating. It will delaminate when the paper contains too much moisture and powder.
Make sure put the material in a low-temperature, dry place.
*Packaging:
Standard export package with carton+pallet.
Surface layer: BOPP
Glue layer: EVA adhesive
*Specification
Gloss
SPECIFICATION | 18mic | 21mic | 24mic | 24mic | 27mic | 30mic | |||
GLOSS | GLOSS | GLOSS | GLOSS | GLOSS | GLOSS | ||||
THICKNESS (mic) | BASE | 12 | 12 | 12 | 15 | 15 | 18 | ||
ADHESIVE | 6 | 9 | 12 | 9 | 12 | 12 | |||
TOTAL | 18 | 21 | 24 | 24 | 27 | 30 | |||
WEIGHT | m2/kg | 60.4 | 51.6 | 45.045 | 45.45 | 40.11 | 36.15 | ||
kg/m2 | 0.01656 | 0.01938 | 0.0222 | 0.022 | 0.02493 | 0.02766 | |||
WIDTH(mm) | 300mm-1800mm | ||||||||
LENGTH(m) | 200m-3000m | ||||||||
PARER CORE | 25mm(1inch),58mm(2.25inches),76mm(3inches) | ||||||||
BONDING | LESS THAN 2 | ||||||||
Matt
SPECIFICATION | 24mic | 27mic | 30mic | |||
MATT | MATT | MATT | ||||
THICKNESS (mic) | BASE | 15 | 15 | 18 | ||
ADHESIVE | 9 | 12 | 12 | |||
TOTAL | 24 | 27 | 30 | |||
WEIGHT | m2/kg | 46.3 | 41 | 37 | ||
kg/m2 | 0.0216 | 0.0244 | 0.0271 | |||
WIDTH(mm) | 300mm-1800mm | |||||
LENGTH(m) | 200m-3000m | |||||
PARER CORE | 25mm(1inch),58mm(2.25inches),76mm(3inches) | |||||
BONDING | LESS THAN 2 | |||||
*Process parameter:
normal | special | |
Temperature | 85 ~ 100ºC | 100 ~ 110 ºC |
Roll Pressure | 8 ~ 15Mpa | 16 ~ 25 Mpa |
Speed | 5 ~ 30 M/min | 5 ~10 M/min |
Lamination Equipment | dry and wet laminator | |
Remarks | Special laminations refer to those with thick ink, dark color, much moisture and large size paper |
*Directions for using BOPP thermal laminating film:
Normal process temperature is 90c-105c, roller pressure and temperature vary with different types of paper, ink and machines.
When using the film for the first time or do other treatment, try a small volume before mass laminating.
Make sure the ink is dry before laminating. It will delaminate when the paper contains too much moisture and powder.
Make sure put the material in a low-temperature, dry place.
*Packaging:
Standard export package with carton+pallet.